Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group OREVAC® 18510 Grafted Maleic Anhydride Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , Anhydride-Modified Polyethylene
Manufacturer Arkema
Trade Name OREVAC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group OREVAC® 18510 Grafted Maleic Anhydride Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OREVAC 18510 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510 is mainly used in pipe coating to have good adhesion performances between an epoxy primer and the HDPE 4206 black or LACQTENE 2006PBK35 from Total Petrochemicals. OREVAC 18510 combined with MD or HDPE and a proper epoxy fulfill the requirement of different application standards such as NFA 49-710 or DIN 30670 when applied in the rules of art.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
ISO 1183
Melt Index of Compound 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ISO 608
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO R 527-2
Elongation at Break 600 %
600 %
ISO R 527-2
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
DSC
Vicat Softening Point 121 °C

@Load 0.999 kg
250 °F

@Load 2.20 lb
ISO 306
Processing Properties Metric English Comments
Zone 1 160 - 180 °C
320 - 356 °F
Zone 2 180 - 200 °C
356 - 392 °F
Zone 3 200 - 220 °C
392 - 428 °F
Zone 4 210 - 230 °C
410 - 446 °F
Die Temperature 220 - 240 °C
428 - 464 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved