Processing Properties Metric English Comments
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 1462Z PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 1462Z is a general purpose, 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.30% glass-fiber, general purposeInformation provid..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2000-3 PBT  (Unverified Data**)
Celanex 2000-3 is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity.. Celanex 2000-3 is a high flow material. Celanex 2000-3 contains an internal..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2402 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2402 MT Natural is an unreinforced PBT with improved flow that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Master Fi..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2404 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2404 MT Natural is an unreinforced PTFE filled PBT with improved friction, sliding, and wear properties that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administra..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3200-2FC PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 3200-2FC is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 3..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3300-2LM PBT, Glass Reinforced  (Unverified Data**)
Celanex 3300-2LM is a 30% glass-filled PBT that is enhanced for improved laser marking graphics. It contains an internal lubricant for enhanced mold release.30% glass-filled PBT, laser markableInfo..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3300LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300LM is a 30% glass reinforced PBT that is enhanced for improved laser marking graphics. 3300LM also offers a superior combination of mechanical, electrical, and thermal properties. This g..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3309HRLM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.30% glass filled PBT, h..
Die Temperature 240 - 260 °C
464 - 500 °F
Celanese Celanex® 3400-2 PBT, 40% Glass Reinforced  (Unverified Data**)
Celanex 3400-2 is a general purpose, 40% glass reinforced polybutylene terephthalate that offers a good combination of mechanical, electrical, and thermal properties. This grade provides outstanding..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 4300FC PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300FC is a toughened, 30% glass reinforced PBT for use in food contact applications.30% glass reinforced PBT for use in food contact applicationsInformation provided by Celanese
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® MT2008 PBT  (Unverified Data**)
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Unfilled PBT for medical ..
Die Temperature 240 - 260 °C
464 - 500 °F
Celanese Vandar® 2500 PBT  (Unverified Data**)
Vandar 2500 is an unfilled polyester alloy which exhibits excellent toughness and impact strength. It is specially designed to offer excellent chemical resistance, good colorability and dimensional ..
Die Temperature 246 - 260 °C
475 - 500 °F
LyondellBasell Alathon® M6080WC High Density Polyethylene
ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c..
Die Temperature 246 - 260 °C
475 - 500 °F
LyondellBasell Petrothene® KR92717 High Density Polyethylene
ApplicationsPETROTHENE KR 92717 is a high molecular weight, high density polyethylene-based compound designed for use in spacer cable insulation and cable jacketing applications. This black compoun..
Die Temperature 220 - 260 °C
428 - 500 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1172D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 1462Z PBT, 30% Glass Reinforced
Celanex 1462Z is a general purpose, 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 1600FC PBT, Unfilled
Celanex 1600FC is a high molecular weight grade of unreinforced polybutylene terephthalate for use in food contact applications that can be used in both extrusion and injection molding applications...
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 1602Z PBT, Unfilled
Celanex 1602Z is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1602Z has an internal lubricant.Information provi..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 1642Z PBT, 20% Glass Reinforced
Celanex 1642Z is a general purpose, 20% fiberglass reinforced PBT with a good balance of mechanical properties and processability.Information provided by Celanese
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 2003HR PBT, Unfilled
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 3201 PBT, 15% Glass Reinforced
Celanex 3201 is a 15% glass reinforced general purpose thermoplastic polyester resin that offers a superior combination of mechanical, electrical, and thermal properties, together with outstanding p..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3201 PBT, 15% Glass Reinforced
Celanex 3201 is a 15% glass reinforced general purpose thermoplastic polyester resin that offers a superior combination of mechanical, electrical, and thermal properties, together with outstanding p..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 602AC PBT, Glass Reinforced
Celanex 602AC is a 10% fiberglass reinforced PBT that has lower warpage and improved impact over standard PBT.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a ..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 3300-2LM PBT, Glass Reinforced
Celanex 3300-2LM is a 30% glass-filled PBT that is enhanced for improved laser marking graphics. It contains an internal lubricant for enhanced mold release. It is a lasermarkable grade available i..
Die Temperature 240 - 260 °C
464 - 500 °F
Celanese RITEFLEX 677 TPC, Unfilled
Riteflex 677 is a thermoplastic polyester elastomer with nominal hardness of 77 shore D and high modulus.Information provided by Celanese
Die Temperature 245 - 260 °C
473 - 500 °F
Average value: 253 °C Grade Count:5
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..
Die Temperature 245 - 260 °C
473 - 500 °F
Celanese Celstran® TPU-GF30-01-US TPU, 30% Glass Reinforced  (Unverified Data**)
30% long strand glass fiber reinforced thermoplastic polyurethane30% long strand glass fiber reinforced thermoplastic polyurethaneCelstran can be processed on a standard injection molding unit.Infor..
Die Temperature 245 - 260 °C
473 - 500 °F
Celanese Celstran® TPU-GF50-01-US TPU, 50% Glass Reinforced  (Unverified Data**)
50% long strand fiber glass reinforced thermoplastic polyurethane50% long strand fiber glass reinforced thermoplastic urethaneCelstran can be processed on a standard injection molding unit.Informati..