Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Griltech Griltex® D 1502E Copolyester Hotmelt Adhesive (Technical Applications)

Category Polymer , Adhesive , Thermoplastic , Polyester, TP
Manufacturer EMS-Griltech
Trade Name Griltex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Griltex® D 1502E Copolyester Hotmelt Adhesive (Technical Applications).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent resistance and dimensional stability of the finished garment. For technical applications, GRILTEX adhesive products are used to optimize the manufacturing process for the production of automotive interior components or parts for other applications. All values were determined on dried pellets.Applications: Filters, Flexible Coatings (flexible)Bonding Properties: Metal, Paper, PolyesterData provided by EMS-Griltech.
Physical Properties Metric English Comments
Viscosity 100000 cP

@Temperature 210 °C
100000 cP

@Temperature 410 °F
2.16 kg load; ISO 1133
Melt Flow 105 g/10 min

@Load 2.16 kg,
Temperature 210 °C
105 g/10 min

@Load 4.76 lb,
Temperature 410 °F
cm<sup>3</sup>/10 min; ISO 1133
Thermal Properties Metric English Comments
Melting Point 180 - 190 °C
356 - 374 °F
DSC
Processing Properties Metric English Comments
Processing Temperature 200 - 230 °C
392 - 446 °F
Lamination Adhesive
Die Temperature 210 - 240 °C
410 - 464 °F
Hotmelt Coating Slot Die
Roll Temperature 200 - 220 °C
392 - 428 °F
Hotmelt Coating Multi Roller
210 - 240 °C
410 - 464 °F
Engraved Roller
Descriptive Properties Value Comments
Crystallization Speed Very Fast
Form of Delivery Granules
Copyright © lookpolymers.com All Rights Reserved