Polymer Property : Feed Temperature = 280 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)  (discontin
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 260 - 280 °C
500 - 536 °F
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, DRY
Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is ..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay TECHNYL® A 225F PA66, DRY
Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct..
Feed Temperature 275 - 280 °C
527 - 536 °F
Solvay TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, DRY
Description: Flame-retardant polyamide 66, 25% glass-fiber reinforced, heat stabilized for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications:..
Feed Temperature 270 - 280 °C
518 - 536 °F
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi..
Feed Temperature 240 - 280 °C
464 - 536 °F
Solvay TECHNYL® C 236SI PA6, DRY
Description: Unreinforced polyamide 6 with high impact strength for injection molding.Available in: Europe and North AmericaProduct Applications: TECHNYL® C 236SI has high impact strength and fle..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay TECHNYL® C 246SI V11 PA6, 11% glass filled, DRY
Description: Polyamide 6, reinforced with 11% of glass fiber, with high impact resistance, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® C 246SI V11 has good mech..
Feed Temperature 275 - 280 °C
527 - 536 °F
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, DRY
Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, at Equilibrium (65% RH)  (discontinu
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM  (discontinued **)<
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)  
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM  (discontinued **)&l
Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, at Equilibrium (65% RH)  
Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)  (discontinued **
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..