PolyChem Alloy PolySlip 254

Category Polymer
Manufacturer PolyChem Alloy
Trade Name PolySlip
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyChem Alloy PolySlip 254.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Slip additive with process aid & anti-block
Processing Properties Metric English Comments
Processing Temperature 170 - 220 °C
338 - 428 °F