Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Suggested Extusion Stock |
S&E Specialty Polymers TufFlex™ GA-94-244B PVC Compound Application: 105°C rated vinyl elastomer for medical wire and cable applications. This product complies with the RoHS Directive.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 171 - 177 °C | 340 - 350 °F | Suggested Stock |
S&E Specialty Polymers TufLite™ GE-01-037C PVC Application: An extra flexible, expandable, PVC based compound suitable for injection molding applications.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ G-2175A PVC Compound Application: A clear, high gloss, PVC based compound designed for profile extrusion applications.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ G-2184M PVC Compound Application: A RoHS compliant, general purpose PVC based compound designed for molding applications.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 171 - 177 °C | 340 - 350 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ G-3468-A PVC Compound Application: A general purpose PVC based extrusion grade compound.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ G-3570 PVC Compound Application: A PVC compound designed for work boot and boat shoe soling applications.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 171 - 177 °C | 340 - 350 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GA-3174 PVC Compound Application: 80°C PVC General Purpose Jacketing compound with high gloss surface.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 171 - 177 °C | 340 - 350 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GA-509-KHA PVC Compound Application: 105°C rated jacketing compound with good low temperature and aging properties.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 160 - 177 °C | 320 - 350 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GM-93-060LT PVC Compound Application: A clear, non-toxic, extrusion compound for food contact use. Compound exhibits excellent low temperature flexibility.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 149 - 177 °C | 300 - 351 °F | Thermoforming surface |
Chevron Phillips Marlex® HHM 5202 Polyethylene, Sheet/Thermoforming Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520.Data provided by the manufacturer |
|||
Processing Temperature | 149 - 177 °C | 300 - 351 °F | Thermoforming surface |
Chevron Phillips Marlex® HHM 5502-01 Polyethylene, Sheet/Thermoforming Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520.Data provided by the manufacturer |
|||
Processing Temperature | 10.0 - 177 °C | 50.0 - 350 °F | Average value: 73.0 °C Grade Count:3 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Processing Temperature | 25.0 - 177 °C | 77.0 - 350 °F | Average value: 125 °C Grade Count:8 |
Overview of materials for Silicone Elastomer, for Thermal Management This property data is a summary of similar materials in the MatWeb database for the category "Silicone Elastomer, for Thermal Management". Each property range of values reported is minimum and maxim.. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 6146-80 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 6161-82 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 6404-78 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 50423 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 5104 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 5108 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 5117-82 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 5131-80 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 574 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 6064 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 6065 LT GL 85 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 143 - 177 °C | 290 - 350 °F | Molding |
Vyncolit INSUL-PLATE™ X-28057-2HT Hole-Fill Powder For Printed Circuit Boards Vyncolit INSUL-PLATE™ Hole-Fill material delivers true reliability and superior performance. This material, in powder form, is specifically suited for Hole-Fill use in glass epoxy, multi-layer and .. |
|||
Processing Temperature | 160 - 177 °C | 320 - 350 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GM-93-060 PVC Compound Application: A clear, non-toxic, extrusion compound for food contact use.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 6134-80 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 6149-80 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
Sylvin Technologies 6150-80 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |