Sylvin Technologies 6404-78 PVC Wire/Cable Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Sylvin Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 6404-78 PVC Wire/Cable Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
10 seconds
Tensile Strength, Ultimate 14.8 MPa
2150 psi
Elongation at Break 450 %
450 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air <= 105 °C
<= 221 °F
Brittleness Temperature -48.0 °C
-54.4 °F
Oxygen Index 21.4 %
21.4 %
Processing Properties Metric English Comments
Processing Temperature 166 - 177 °C
330 - 350 °F
Recommended Stock Temperature