Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Processing Temperature = 340 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 171 - 177 °C
340 - 350 °F
Suggested Stock
S&E Specialty Polymers TufLite™ GE-01-037C PVC
Application: An extra flexible, expandable, PVC based compound suitable for injection molding applications.Information provided by S&E Specialty Polymers
Processing Temperature 171 - 182 °C
340 - 360 °F
Suggested Stock
S&E Specialty Polymers TufTech™ GA-1038 Natural MA PVC Compound
Application: A RoHS compliant, 60°C PVC wire and cable compound. Material is suitable for 60°C and 75°C SVT and SJT insulation.Information provided by S&E Specialty Polymers
Processing Temperature 171 - 199 °C
340 - 390 °F
Average value: 185 °C Grade Count:13
Overview of materials for Styrenic TPE  (Unverified Data**)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe..
Processing Temperature 171 - 182 °C
340 - 360 °F
Thermoforming Surface Temp
Chevron Phillips Marlex® HHM 5502-04BN HDPE Hexene Copolymer  (discontinued **)
This resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergents. Meets ASTM D4976 - PE 235. ASTM D1248 - Type III, Class A, Cat..
Processing Temperature 171 - 204 °C
340 - 399 °F
Blow Molding Stock
Chevron Phillips Marlex® HHM 5502-04BN HDPE Hexene Copolymer  (discontinued **)
This resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergents. Meets ASTM D4976 - PE 235. ASTM D1248 - Type III, Class A, Cat..
Processing Temperature 171 - 193 °C
340 - 379 °F
Molding temperature
Cookson Group Plaskon® 3200LS Mineral Filled Novolac Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability under very stringent testing. This material is designed to minimize stress on the encapsulated ..
Processing Temperature 171 °C
340 °F
Gel time is 350-500 min. at 171°C.
Huntsman Kerimid 8292 N-75 Resin
Comments/Applications: Kerimid 8292 supplies as a 75% by weight solution in MEK.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Processing Temperature 171 - 182 °C
340 - 360 °F
Recommended Stock Temperature
Sylvin Technologies 6160-90 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Processing Temperature 171 - 182 °C
340 - 360 °F
Recommended Stock Temperature
Sylvin Technologies 6140-90 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Processing Temperature 171 - 226 °C
340 - 439 °F
Chevron Phillips Marlex® EHM 6007 High Density Polyethylene
High Density PolyethyleneCustomer Benefits: A blow molding grade rein that offers a high quality product for those critical food packaging jobs and good impact strength and stiffness.Applications: L..
Processing Temperature 171 - 182 °C
340 - 360 °F
Thermoforming Surface
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer
High Density Ethylene Hexene-1 CopolymerCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of products. Has exce..
Processing Temperature 171 - 197 °C
340 - 387 °F
DSM Biomedical Elasthane™ 80A Thermoplastic Polyether Polyurethane (TPU)
A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility Elasthane™ TPU exhibits outstanding hydrolytic stabilit..
Processing Temperature 171 - 182 °C
340 - 360 °F
Thermoforming Surface
Chevron Phillips Marlex® HHM 5202-02 BN High Density Ethylene Hexene-1 Copolymer
High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers ..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2740S-70A  Unsaturated Styrenic Elastomer (SEBS) 70 Shore A - SEBS  (discont
70 Shore A - SEBSComments:70-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2799S X 89622 C  Styrenic Thermoplastic Elastomer (TES) Thermally Conductive - Electrically Conductive - SEBS
Thermally Conductive - Electrically Conductive - SEBS Comments:Thermally ConductiveElectrically ConductiveSEBS TypeUnless otherwise specified, all data listed is for natural or black colored materia..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2800B-50A  Thermoplastic Vulcanizate Elastomer (TPV) 50 Shore A  (discontinu
50 Shore AComments:50-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2800B-55A  Thermoplastic Vulcanizate Elastomer (TPV) 55 Shore A  (discontinu
55 Shore AComments:55-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2800B-80A  Thermoplastic Vulcanizate Elastomer (TPV) 80 Shore A  (discontinu
80 Shore AComments:80-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2800B-50A FR  Thermoplastic Vulcanizate Elastomer (TPV) 50 Shore A - Flame Retardant
50 Shore A - Flame RetardantComments:50-A DurometerFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information pr..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2800B-30D FR  Thermoplastic Vulcanizate Elastomer (TPV) 30 Shore D - Flame Retardant
30 Shore D - Flame RetardantComments:30-D DurometerFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information pr..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2800B-30D HF  Thermoplastic Vulcanizate Elastomer (TPV) 30 Shore D - High Flow &n
30 Shore D - High FlowComments:30-D DurometerHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RT..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2800B-50D HF  Thermoplastic Vulcanizate Elastomer (TPV) 50 Shore D - High Flow &n
50 Shore D - High FlowComments:50-D DurometerHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RT..
Processing Temperature 171 - 182 °C
340 - 360 °F
Recommended Stock Temperature
Sylvin Technologies 6148-90 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2740U-60A  Saturated Styrenic Elastomer (SBS) 60 Shore A  (discontinued **)&
60 Shore AComments:60-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2740U-70A  Saturated Styrenic Elastomer (SBS) 70 Shore A  (discontinued **)&
70 Shore AComments:70-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2740U-80A  Saturated Styrenic Elastomer (SBS) 80 Shore A  (discontinued **)&
80 Shore AComments:80-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2740S-60A  Unsaturated Styrenic Elastomer (SEBS) 60 Shore A - SEBS  (discont
60 Shore A - SEBSComments:60-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company ESD C 2800B-90A  Thermoplastic Vulcanizate Elastomer (TPV) Conductive - 90 Shore A &n
Conductive - 90 Shore AComments:ConductiveESD Protection90-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Informatio..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2800B-60A  Thermoplastic Vulcanizate Elastomer (TPV) 60 Shore A  (discontinu
60 Shore AComments:60-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Processing Temperature 171 - 199 °C
340 - 390 °F
RTP Company RTP 2800B-55A HF  Thermoplastic Vulcanizate Elastomer (TPV) 55 Shore A - High Flow &n
55 Shore A - High FlowComments:55-A DurometerHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RT..