S&E Specialty Polymers TufFlex™ GA-94-244B PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufFlex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufFlex™ GA-94-244B PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: 105°C rated vinyl elastomer for medical wire and cable applications. This product complies with the RoHS Directive.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 65.0

@Time 15.0 sec
65.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 14.5 MPa
2100 psi
ASTM D412
14.79 MPa

@Temperature 136 °C,
Time 605000 sec
2145 psi

@Temperature 277 °F,
Time 168 hour
Air Oven Aged
Elongation at Break 360 %
360 %
ASTM D412
288 %

@Treatment Temp. 136 °C,
Time 605000 sec
288 %

@Treatment Temp. 277 °F,
Time 168 hour
Air Oven Aged
Processing Properties Metric English Comments
Processing Temperature 166 - 177 °C
330 - 350 °F
Suggested Extusion Stock