Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 41.1 °C @Thickness 3.18 mm |
106 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L0313 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.1 °C @Thickness 3.18 mm |
106 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L8230 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | |
LyondellBasell Lupolen® 3652 D SW 00413 MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | |
LyondellBasell Lupolen® 3822 D GB 00350 MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | |
LyondellBasell Lupolen® 4152 D SW 00413 HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | |
LyondellBasell Lupolen® UHM 201 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | |
LyondellBasell Lupolen® UHM 301 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C @Thickness 3.20 mm |
106 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp TH0450D LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C @Thickness 3.20 mm |
106 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific) LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | Method A; ASTM D-648 |
Chevron Phillips Marlex® HMN TR-935/935G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationExcellent impac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | ASTM D648 |
DSM Somos® GP Plus 14122 Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.1 °C | 106 °F | ASTM D648 |
ExxonMobil HDPE HD 8660.29 High Density Polyethylene Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.1 °C | 106 °F | ASTM D648 |
ExxonMobil HDPE HD P8660.29 High Density Polyethylene Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | ASTM D648 |
ExxonMobil HD 8660.29 Rotational Molding Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | ASTM D648 |
ExxonMobil HDP8660.29 Rotational Molding Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® HTR8068 Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Flame Retardant Polyester Elastomer Developed for Extrusion and Injection Molding Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | ASTM D648 |
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic High clarity plastic for a multitude of applicationsFeaturesClear and transparentRigid and toughGreat for headlamps, bottles and transparent assembliesExcellent humidity/moisture resistanceAll infor.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | |
Arkema Group Rilsan® MA 4411 Nylon 12, Flexible Tubing Grade (Dry) Designation ISO 1874-PA12-HI,EHL,22-003Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit fo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | ASTM-D648 |
Braskem ML3601U LLDPE Rotomolding Polyethylene The resin ML3601U is a linear low-density polyethylene, 1-hexene based, with excellent environmental stress cracking resistance and high impact strength. It contains long term UV8 stabilization and .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | ASTM-D648 |
Braskem RC35U4 LLDPE Rotomolding Polyethylene The resin RC35U4 is a linear low-density polyethylene, 1-butene based, with high stiffness and an adequate balance of processability and environmental stress cracking resistance. It contains long te.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | ISO 75-2/AF |
Addiplast Addilene J 380 Polypropylene Copolymer High impact strength, high elongation at breakInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | |
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | ASTM D648 |
Lucent Polymers TPO-10T Thermoplastic Polyolefin, 10% Mineral Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 °C | 106 °F | ISO 75 |
LyondellBasell Hifax™ CA186 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, excellent paintability and paint durability, good processabi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 - 99.0 °C | 106 - 210 °F | Average value: 53.7 °C Grade Count:20 |
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Rotational Molding Grade". Each property range of values reported is m.. |