Material Notes:
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.013 cm/cm

@Thickness 3.17 mm
0.013 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Strength 29.0 MPa
4210 psi
ASTM D790
Flexural Modulus 0.772 GPa
112 ksi
ASTM D790
Izod Impact, Notched 9.99 J/cm

@Thickness 3.17 mm
18.7 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °C
106 °F
ASTM D648