LyondellBasell Lupolen® UHM 301 MDPE, Ultra-High Molecular Weight

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Ultra High Molecular Weight
Manufacturer LyondellBasell
Trade Name Lupolen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Lupolen® UHM 301 MDPE, Ultra-High Molecular Weight.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this material contains no other additives.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Physical Properties Metric English Comments
Density 0.929 g/cc
0.0336 lb/in³
Water Absorption 0.10 %
0.10 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
Elongation at Break >= 50 %
>= 50 %
Elongation at Yield 14 %
14 %
Tensile Modulus 0.725 GPa
105 ksi
Tensile Creep Modulus, 1 hour 260 MPa
37700 psi
Tensile Creep Modulus, 1000 hours 200 MPa
29000 psi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 210 µm/m-°C

@Temperature 20.0 °C
117 µin/in-°F

@Temperature 68.0 °F
Melting Point 136 °C
277 °F
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °C
106 °F
Vicat Softening Point 81.0 °C
178 °F
Flammability, UL94 HB

@Thickness 0.400 mm
HB

@Thickness 0.0157 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 600 V
600 V