LyondellBasell Lupolen® 3822 D GB 00350 MDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Molded
Manufacturer LyondellBasell
Trade Name Lupolen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Lupolen® 3822 D GB 00350 MDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Physical Properties Metric English Comments
Density 0.938 g/cc
0.0339 lb/in³
Water Absorption 0.010 %
0.010 %
Melt Flow 0.26 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.26 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
Elongation at Break >= 50 %
>= 50 %
Elongation at Yield 8.0 %
8.0 %
Tensile Modulus 0.700 GPa
102 ksi
Tensile Impact Strength 200 kJ/m²
95.2 ft-lb/in²
Thermal Properties Metric English Comments
Melting Point 128 °C
262 °F
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C
156 °F
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °C
106 °F
Vicat Softening Point 65.0 °C
149 °F
Flammability, UL94 HB

@Thickness 0.400 mm
HB

@Thickness 0.0157 in
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm