Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil HDPE HD P8660.29 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HDPE HD P8660.29 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance of low temperature toughness, creep resistance, stiffness, ESCR and tear properties.Availability: Latin America, North America and South America Additive: Long Term UV-15 Stabilizer: YesApplications: Industrial ProductsIntermediate Bulk ContainersLarge Agricultural TanksInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.942 g/cc
0.0340 lb/in³
ASTM D4883
ESCR 100% Igepal® 550 hour
550 hour
F50; ASTM D1963A
ESCR 10% Igepal® 50 hour
50 hour
F50; ASTM D1963A
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
(2.0 in/min); ASTM D638
Elongation at Yield 20 %
20 %
ASTM D638
Flexural Modulus, 1% Secant 896 MPa
130000 psi
ASTM D790B
Impact Test 244 J

@Thickness 6.35 mm
180 ft-lb

@Thickness 0.250 in
ARM
108 J

@Thickness 3.17 mm,
Temperature -40.0 °C
80.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
Thermal Properties Metric English Comments
Melting Point <= 264 °C
<= 507 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 67.2 °C
153 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 41.1 °C
106 °F
ASTM D648
Users viewing this material also viewed the following: