Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 41.1 °C @Thickness 3.18 mm |
106 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L0313 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.1 °C @Thickness 3.18 mm |
106 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L8230 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.1 °C | 106 °F | ASTM D648 |
ExxonMobil HDPE HD 8660.29 High Density Polyethylene Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.1 °C | 106 °F | ASTM D648 |
ExxonMobil HDPE HD P8660.29 High Density Polyethylene Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |