Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.89 - 17.2 GPa | 1000 - 2500 ksi | Average value: 9.08 GPa Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flexural Modulus | 12.4 - 17.2 GPa | 1800 - 2500 ksi | Average value: 14.6 GPa Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Flexural Modulus | 4.48 - 17.2 GPa | 650 - 2500 ksi | Average value: 7.75 GPa Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Flexural Modulus | 1.21 - 17.2 GPa | 175 - 2500 ksi | Average value: 7.83 GPa Grade Count:15 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Flexural Modulus | 7.90 - 17.2 GPa | 1150 - 2500 ksi | Average value: 13.9 GPa Grade Count:111 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Flexural Modulus | 6.55 - 17.2 GPa | 950 - 2500 ksi | Average value: 11.1 GPa Grade Count:7 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Flexural Modulus | 4.83 - 17.2 GPa | 700 - 2500 ksi | Average value: 10.4 GPa Grade Count:24 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |