This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.10 - 1.26 g/cc
0.0397 - 0.0455 lb/in³
Average value: 1.17 g/cc Grade Count:6
Filler Content 10.0 - 40.0 %
10.0 - 40.0 %
Average value: 21.3 % Grade Count:4
Linear Mold Shrinkage 0.00100 - 0.00200 cm/cm
0.00100 - 0.00200 in/in
Average value: 0.00144 cm/cm Grade Count:6
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.2 - 103 MPa
8000 - 15000 psi
Average value: 74.7 MPa Grade Count:6
Elongation at Break 0.000 - 2.00 %
0.000 - 2.00 %
Average value: 1.33 % Grade Count:6
Modulus of Elasticity 8.27 - 20.7 GPa
1200 - 3000 ksi
Average value: 10.9 GPa Grade Count:6
Flexural Yield Strength 89.6 - 138 MPa
13000 - 20000 psi
Average value: 109 MPa Grade Count:6
Flexural Modulus 6.89 - 17.2 GPa
1000 - 2500 ksi
Average value: 9.08 GPa Grade Count:6
Izod Impact, Notched 0.534 - 0.801 J/cm
1.00 - 1.50 ft-lb/in
Average value: 0.596 J/cm Grade Count:6
Izod Impact, Unnotched 1.07 - 2.14 J/cm
2.00 - 4.00 ft-lb/in
Average value: 1.74 J/cm Grade Count:6
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 93.3 - 149 °C
200 - 300 °F
Average value: 127 °C Grade Count:6
Flammability, UL94 HB - V-1
HB - V-1
Grade Count:6
Electrical Properties Metric English Comments
Electrical Resistivity 1000 - 10000 ohm-cm
1000 - 10000 ohm-cm
Average value: 2500 ohm-cm Grade Count:6
Processing Properties Metric English Comments
Processing Temperature 232 - 282 °C
450 - 540 °F
Average value: 257 °C Grade Count:6
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Average value: 79.4 °C Grade Count:6
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:6