Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.21 GPa | 175 ksi | Tangent; ASTM D790 |
RheTech Products FT4650-583UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 20-1202 Description: Random Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Cellular E2001 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 3 pt. Tangent; ASTM D790 |
Chevron Phillips HiD® 9062 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Formosa Plastics Formolene® LH6008 Injection Molding HDPE
(discontinued **) HomopolymerApplications: Totes, cases, crates, over-caps, toysFormolene LH6008 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Admi.. |
|||
Flexural Modulus | 1.21 - 17.2 GPa | 175 - 2500 ksi | Average value: 7.83 GPa Grade Count:15 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Flexural Modulus | 1.21 GPa | 176 ksi | ASTM D790 |
LyondellBasell Petrothene® LR734001 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Flexural Modulus | 1.21 GPa | 176 ksi | ASTM D790 |
LyondellBasell Petrothene® LR734001 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Flexural Modulus | 1.21 GPa | 176 ksi | ASTM D790 |
LyondellBasell Petrothene® LR734011 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Flexural Modulus | 1.21 GPa | 176 ksi | ASTM D790 |
LyondellBasell Petrothene® LR734045 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
M. Holland Company CP200 Polypropylene Impact Copolymer Impact copolymerMedium impact resistanceLow temperature impact resistanceApplications: Appliance componentsConsumer ApplicationsHousehold goodsInformation provided by M. Holland |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Tangent-Method 1; ASTM D790 |
Ineos T50-1000 HDPE Copolymer T50-1000 is a high density polyethylene copolymer. It has a narrow molecular weight distribution and provides injection molded parts with an excellent balance of properties and processing for most g.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Multibase Multi-Flamâ„¢ 0302 PP NH Polypropylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingCoextrusionExtrusionUses:TubingPipingFurnitureInformation provided by Multibase |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES HiFill® HDPE UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTU PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency, UV cut, and superior cleanliness for advanced semiconductor packaging applications |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES Luriblend® PA4/6 HS TL15 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedUL File Number: E157318Information provided by TP Composites, Inc... |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D709A |
Styron INSPIREâ„¢ TF1302 Thermoplastic Polyolefin Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES HiFill® HDPE Availability: North AmericaForms: PelletsProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp 2Z004 FP-E (EFTE) LNP* 2Z004 is a compound based on Ethylenetetrafluoroethylene (ETFE) containing Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D 790 |
Total 50100.1 HDPE blow molding Applications: Agricultural chemical tanks, portable fuel containers, industrial parts, pallets, large foam parts, food packaging. Blow Molding Stock Temperature 370 – 450 ºF Extrusion melt tempera.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 2520N Injection Molding Polypropylene Impact Copolymer for Injection MoldingFormolene® 2520N is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dimensional stabili.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 6144O Impact Copolymer Polypropylene Impact Copolymer for Appliance Applications Formolene® 6144O is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dimensional s.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Lubrizol ESTALOC® 59104 Ester-Type, Reinforced Engineering Thermoplastic Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impactUses: Injection Molding Available in Americas and AsiaInformation provided by Lubrizol |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI4007G Impact Copolymer Polypropylene Description: Extra high izod impact, superior low temperature drop impact.Applications: Suggested uses include profiles, tubing, squeeze bottles. UL temperature index of 100ºC.Process: Injection Mo.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI4015F Impact Copolymer Polypropylene Description: Superior balance of stiffness and impact strength. Applications: Suggested uses include extrusion applications requiring good impact strength. Process: Extrusion. This resin meets the .. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Amco PRIMATOP HDPE 080960 Injection Molding Polyethylene HDPE 080960 features high stiffness, maximum toughness, good top loading capability, and high surface gloss. Applications include tote boxes and beverage crates.Former A-Top Polymers product; part o.. |
|||
Flexural Modulus | >= 1.21 GPa | >= 175 ksi | tangent; ASTM D790 |
S&E Specialty Polymers GPP1001V0M-HCO PP Application: A polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications. It affords medium impact resistance with a high level of flam.. |