Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
Quadrant EPP Ketron® CM 1030HT PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
Polymer Resources TP-GFMF2 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced Polybutylene Terephthalate, 40% Glass/Mineral ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Flexural Modulus | 7.92 GPa | 1150 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL16E PC (Asia Pacific) LNP* Lubricomp* DFL16E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Easy Molding. |
|||
Flexural Modulus | 7.91 GPa | 1150 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36L PA6.12 LNP* LUBRICOMP* IFL36L is a compound based on Nylon 6/12 containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Low Extractable, Wear Resistant. |
|||
Flexural Modulus | 7.90 GPa | 1150 ksi | ISO 178 |
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, DRY Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl.. |
|||
Flexural Modulus | 7.92 GPa | 1150 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP SFP36 PA12 LNP* LUBRICOMP* SFP36 is a compound based on Nylon 12 resin containing 30% Glass Fiber 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 7.90 GPa | 1150 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WFI18 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFI18 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Silicone. |
|||
Flexural Modulus | 7.92 GPa | 1150 ksi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Flexural Modulus | 7.92 GPa | 1150 ksi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+PS LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Flexural Modulus | 7.90 GPa | 1150 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RFC16 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RFC16 is a compound based on PA 66 resin containing Glass Fiber, Carbon Fiber. Added features include: Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy Information provided by A. Schulman. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
Chase Plastics CP Pryme® PC130R Polycarbonate, 30% Glass Fiber Reinforced Features: Good mold releaseForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 7.95 GPa | 1150 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 226 40% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy Information provided by A. Schulman. |
|||
Flexural Modulus | 7.95 GPa | 1150 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 226 40% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
Flexural Modulus | 7.95 GPa | 1150 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 226 40% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFPC-30 30% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy Information provided by A. Schulman. |
|||
Flexural Modulus | 7.90 GPa | 1150 ksi | ISO 178 |
Eurostar Star L PA6 30V D51 PA6, Glass Filled, Injection Molding Star L PA6 30V D51 is a PTFE Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 7.90 GPa | 1150 ksi | ASTM D790 |
Ashley Polymers Ashlene® 630-33G Nylon 6, 33% Glass Reinforced Nylon 6, 33% glass reinforced resin.Data provided by the manufacturer |
|||
Flexural Modulus | 7.90 GPa | 1150 ksi | ASTM D790 |
Chem Polymer Chemlon 233 G Nylon 6, 33% Glass Fiber Reinforced A 33% glass fiber reinforced nylon 6 offering excellent high temperature performance, dimensional stability, tensile strength and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Modulus | 7.90 GPa | 1150 ksi | ASTM D790 |
Chem Polymer Durlex 730 G PBT, 30% Glass Fiber Reinforced A lubricated 30% glass reinforced PBT offering a balance of dimensional stability, tensile strength and high temperature performance.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Modulus | 7.90 GPa | 1150 ksi | ISO 178 |
Polyplastic Armamid® PA6 GF 30-2HSM-902 Nylon, 30% Glass Filled Heat stabilizedInformation provided by PolyPlastic Group. |
|||
Flexural Modulus | 7.94 GPa | 1150 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EFL34HL PEI LNP LUBRICOMP* EFL34HL is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable. |
|||
Flexural Modulus | 7.92 GPa | 1150 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON LX00797C PEEK LNP* STAT-KON* LX00797C is a compound based on Polyetheretherketone containing Proprietary Filler(s). Added features of this material include: ristics of this grade are: Clean Compounding System, .. |