Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 16.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.110 GPa
16.0 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE G 7150 BLK
Multi-Flex® G 7150 is based on Shell's Kraton G technology, manufactured under the license of Shell. Multibase certifies that his product has been formulated with the same ingredients as manufactu..
Flexural Modulus 0.110 GPa
16.0 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Flex® TPO D-3120
Multi-Flex® TPO D-3120 is a compound for automotive applications replacing Himont's 7023. The burn rate is 0.87 in/min; ASTM FM VSS 30.Data provided by Multibase.
Flexural Modulus 0.110 GPa
16.0 ksi
ISO 178
Polimeri Europa Riblene® MT 10 Low Density Polyethylene - Injection Molding
Riblene MT 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 are highly flexible.Main Applications: Riblene MT 10 is suitable for injection mo..
Flexural Modulus 0.110 GPa
16.0 ksi
ISO 178
Polimeri Europa Riblene® MV 10 Low Density Polyethylene - Injection Molding
Riblene MV 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 are highly flexible.Main Applications: Riblene MV 10 is ideal for injection moldi..
Flexural Modulus 0.110 GPa
16.0 ksi
ISO 178
Polimeri Europa Riblene® MV 10 R Low Density Polyethylene - Injection Molding
Riblene MV 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 R are highly flexible.Main Applications: Riblene MV 10 R is ideal for injection..
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
Rotuba MH Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Flexural Modulus 0.110 GPa
16.0 ksi
ISO 178
Polimeri Europa Riblene® MT 10 R Low Density Polyethylene - Injection Molding
Riblene MT 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 R are highly flexible.Main Applications: Riblene MT 10 R is suitable for inject..
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical  (discontinued **)
This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r..
Flexural Modulus 0.110 GPa
16.0 ksi
1% secant at 0.05 in/min; ASTM D790A
LyondellBasell Adflexâ„¢ KS-084P TPO Resin
Primary Processing Method: ExtrusionKey Features: high melt flow, low modulus, impact resistant thermoplastic olefin, resin, good heat sealability, outstanding puncture resistance, excellent balance..
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCA871 PPE-TPE (Asia Pacific)
Halogen-free flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as insulation and cable jacket. Flame retardant performance and mechanical properties capable..
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCA871 PPE-TPE (Asia Pacific)
Halogen-free flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as insulation and cable jacket. Flame retardant performance and mechanical properties capable..
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCD801AU PPE-TPE (Asia Pacific)
Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r..
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP821 PPE-TPE
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Asia Pacific)
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East)
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP921A PPE-TPE
Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect..
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCP921A PPE-TPE
Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect..
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Asia Pacific)
Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect..
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Asia Pacific)
Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect..
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Europe-Africa-Middle East)
Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect..
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Europe-Africa-Middle East)
Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect..
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
Teknor Apex TEKRON® 4300LM-P86-1 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
Toyobo PELPRENE™ P46D-01 Polyester TPE, High Viscous, High Durability
Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo.
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
DuPont Keldax® 6798 Filled Thermoplastic Ethylene Polymer
A low fog filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailabil..
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
Covestro Bayflex® XGT-16 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Flexural Modulus 0.110 GPa
16.0 ksi
Dow AFFINITY™ SM 1300 Polyolefin Plastomer
AFFINITY® SM 1300 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in high clarity durable injection molded industrial and consumer goods and compression molded closu..
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
3D Systems VisiJet M100 3-D Printer Model Material
The InVision SR (standard resolution) 3-D printer delivers key advantages compared to other 3-D modeling technologies — superior model quality, durable photopolymer materials, surface finish and fe..
Copyright © lookpolymers.com All Rights Reserved