Rotuba MH Cellulose Acetate

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Cellulose Acetate, Molded
Manufacturer Rotuba
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rotuba MH Cellulose Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Property values at 50% RH.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Water Absorption 2.3 %
2.3 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 66
66
ASTM D785
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ASTM D638
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 43 %
43 %
ASTM D638
Flexural Yield Strength 39.0 MPa
5660 psi
ASTM D790
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
Izod Impact, Notched 2.35 J/cm
4.40 ft-lb/in
ASTM D256
0.640 J/cm

@Temperature -40.0 °C
1.20 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 150 °C
302 °F
Flow temperature, ASTM D569
Processing Properties Metric English Comments
Processing Temperature 200 °C
392 °F
Center barrel temperature