Teknor Apex TEKRON® 4300LM-P86-1 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name TEKRON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex TEKRON® 4300LM-P86-1 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
+/- 0.02; ASTM D792
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
24 hours
0.017 cm/cm
0.017 in/in
24 hours + 30 min at 93°C
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
24 hours
0.015 cm/cm
0.015 in/in
24 hours + 30 min. at 93°C
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
15 second delay. +/-3; ASTM D2240
Tensile Strength, Yield 10.20 MPa
1479 psi
ASTM D412
Elongation at Break 660 %
660 %
ASTM D412
100% Modulus 0.00593 GPa
0.860 ksi
ASTM D412
300% Modulus 0.007074 GPa
1.026 ksi
ASTM D412
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746
Flame Spread 18.3 mm/min
0.720 in/min
Pass: Burn Rate- Max 100; FMVSS 302
Descriptive Properties Value Comments
Fogging 98.3, 3 hours at 100°C. (SAE-J1756)