3D Systems VisiJet M100 3-D Printer Model Material

Category Polymer , Rapid Prototyping Polymer , Thermoplastic
Manufacturer 3D Systems Corporation
Trade Name VisiJet
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3D Systems VisiJet M100 3-D Printer Model Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The InVision SR (standard resolution) 3-D printer delivers key advantages compared to other 3-D modeling technologies — superior model quality, durable photopolymer materials, surface finish and feature detail, and the ability to build complex models or patterns. Choose from five model material colors - black, blue, red, grey, and white. Reported here is preliminary tech data for the cured plastic models.Information provided by 3D Systems Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
Cured
Ash 0.010 %
0.010 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.0 MPa
3480 psi
ASTM D638
Elongation at Break 15.6 %
15.6 %
ASTM D638
Tensile Modulus 0.7750 GPa
112.4 ksi
ASTM D638
Flexural Strength 42.1 MPa
6100 psi
ASTM D790
Flexural Modulus 0.110 GPa
16.0 ksi
ASTM D790
Izod Impact, Notched 0.133 J/cm
0.250 ft-lb/in
ASTM D256