Dow AFFINITY™ SM 1300 Polyolefin Plastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ SM 1300 Polyolefin Plastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY® SM 1300 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in high clarity durable injection molded industrial and consumer goods and compression molded closure liners or gaskets. It exhibits excellent optics and flexibility, and allows the use of hot runner molds to enhance production automation. Its low specific gravity can help control resin and production costs, while reducing the weight of end products.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
Melt Flow 30 g/10 min

@Load 2.16 kg
30 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 7.
Mechanical Properties Metric English Comments
Hardness, Shore D 94
94
Tensile Strength, Yield 5.90 MPa
856 psi
Elongation at Break 940 %
940 %
Modulus of Elasticity 0.0950 GPa
13.8 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 0.110 GPa
16.0 ksi
Thermal Properties Metric English Comments
Vicat Softening Point 74.0 °C
165 °F