LyondellBasell Adflexâ„¢ KS-084P TPO Resin

Category Polymer , Thermoplastic
Manufacturer LyondellBasell
Trade Name Adflex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Adflexâ„¢ KS-084P TPO Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primary Processing Method: ExtrusionKey Features: high melt flow, low modulus, impact resistant thermoplastic olefin, resin, good heat sealability, outstanding puncture resistance, excellent balance of flexibility, excellent low temperature impact resistance, excellent chemical and environmental stress-cracking resistance, FDA acceptableApplications: extrusion coatings on a variety of substrates, film, fiberMeets FDA requirements in 21 CFR 177.2600 for rubber articles with repeated use applications. The final item is subject to extraction requirements in 21 CFR 177.2600.Description: Adflex KS-084P high melt flow, low modulus thermoplastic olefin resin is designed for many commercial and industrial extrusion applications. It is based on material produced from Montell's proprietary Catalloy process. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for resins in rubber articles for repeated use applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.880 g/cc
0.0318 lb/in³
ASTM D792B
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 44
44
ASTM D2240
Tensile Strength, Yield 6.00 MPa
870 psi
ASTM D638
Elongation at Break 670 %
670 %
ASTM D638
Elongation at Yield 23 %
23 %
ASTM D638
Flexural Modulus 0.110 GPa
16.0 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched NB
NB
ASTM D256A