Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Riblene® MT 10 R Low Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Riblene® MT 10 R Low Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Riblene MT 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 R are highly flexible.Main Applications: Riblene MT 10 R is suitable for injection molding applications. Riblene MT 10 R is recommended for low thickness articles, artificial flowers and masterbatches.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.917 g/cc
0.917 g/cc
ISO 1183
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 43
43
ISO 868/A
Tensile Strength, Yield 9.00 MPa
1310 psi
ISO 527
Flexural Modulus 0.110 GPa
16.0 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 106 °C
223 °F
Internal method
Vicat Softening Point 82.0 °C

@Load 1.00 kg
180 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -10.0 °C
<= 14.0 °F
ASTM D746
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved