Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.20 - 3.38 GPa | 174 - 490 ksi | Average value: 2.60 GPa Grade Count:18 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Flexural Modulus | 1.36 - 3.38 GPa | 198 - 490 ksi | Average value: 2.11 GPa Grade Count:71 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Flexural Modulus | 1.86 - 3.38 GPa | 270 - 490 ksi | Average value: 2.76 GPa Grade Count:10 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |