Polimeri Europa Eraclene® BB 76 High Density Polyethylene - Blow Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Eraclene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Eraclene® BB 76 High Density Polyethylene - Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eraclene BB 76 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 30 liters.Eraclene BB 76 combines an excellent stress cracking resistance with a good rigidity and a high impact strength. For its overall characteristics, Eraclene BB 76 can be used to produce containers able to achieve UN homologation.Main Applications: Eraclene BB 76 is the ideal resin for packaging of household and industrial chemicals, detergents, fertilizers, adhesives and pesticides. Eraclene BB 76 can also be extruded to obtain profiles and sheets.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.952 g/cc
0.952 g/cc
ISO 1183
Environmental Stress Crack Resistance >= 750 hour
>= 750 hour
ISO 22088
Melt Flow 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ISO 868/A
Tensile Strength at Break 30.0 MPa
4350 psi
ISO 527
Tensile Strength, Yield 27.0 MPa
3920 psi
ISO 527
Elongation at Break >= 600 %
>= 600 %
ISO 527
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Izod Impact, Notched 2.50 J/cm
4.68 ft-lb/in
ISO 180/A
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
Internal method
Vicat Softening Point 126 °C

@Load 1.00 kg
259 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746