Material Notes:
An economy grade, unplasticized Nylon 11 for extrusion applications. Also available is L935H, same with UV and heat stabilizer.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Moisture Absorption at Equilibrium 1.1 %
1.1 %
65% RH; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ATSM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
ASTM D790
Izod Impact, Notched 0.910 J/cm
1.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 191 °C
376 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C
115 °F
ASTM D648