Ensinger ENSITEP® PBT Polybutylene Terephthalate - Extruded Products  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Extrusion Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger ENSITEP® PBT Polybutylene Terephthalate - Extruded Products  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ENSITEP BT is an unreinforced thermoplastic polyester derived from polybutylene terephthalate. Its excellent wear and impact resistance, low coefficient of friction, high flexural modulus, and superior dimensional stability make it a versatile material for designing mechanical and electro-mechanical parts. Because ENSITEP BT has no centerline porosity, the possibility of fluid absorption and leakage is virtually eliminated.Uses: ENSITEP's superior wear resistance and lack of centerline porosity give it an advantage over other materials for applications involving solvents, chemicals, and food products. ENSITEP is also used in water purification systems, printing equipment, textile components, food-handling equipment, and valves.Ensitep grades have been replaced by TecapetInformation supplied by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Water Absorption 0.080 %
0.080 %
24 hrs.; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 72
72
ASTM D785
Tensile Strength at Break 59.9 MPa
8690 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Modulus of Elasticity 2.86 GPa
415 ksi
ASTM D638
Flexural Yield Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.28 GPa
331 ksi
ASTM D790
Shear Modulus 1.04 GPa
151 ksi
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 83.5 µm/m-°C

@Temperature 20.0 °C
46.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.30 J/g-°C
0.311 BTU/lb-°F
Thermal Conductivity 0.210 W/m-K
1.46 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 254 °C
489 °F
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
309 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.2

@Frequency 100 Hz
3.2

@Frequency 100 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm

@Thickness 3.17 mm
399 kV/in

@Thickness 0.125 in
short term; ASTM D149
Dissipation Factor 0.0010

@Frequency 100 Hz
0.0010

@Frequency 100 Hz
ASTM D150