Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 3.92 - 131 MPa | 569 - 19000 psi | Average value: 47.4 MPa Grade Count:273 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Flexural Yield Strength | 103 - 131 MPa | 14900 - 19000 psi | Average value: 107 MPa Grade Count:10 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report.. |
|||
Flexural Yield Strength | 82.7 - 131 MPa | 12000 - 19000 psi | Average value: 93.5 MPa Grade Count:35 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Flexural Yield Strength | 50.0 - 131 MPa | 7250 - 19000 psi | Average value: 81.2 MPa Grade Count:108 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Yield Strength | 68.0 - 131 MPa | 9860 - 19000 psi | Average value: 100 MPa Grade Count:5 |
Overview of materials for Polycarbonate/Styrenic Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a.. |
|||
Flexural Yield Strength | 13.8 - 131 MPa | 2000 - 19000 psi | Average value: 75.1 MPa Grade Count:28 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Flexural Yield Strength | 70.0 - 131 MPa | 10200 - 19000 psi | Average value: 105 MPa Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu.. |