Material Notes:
High impact, good flowability and heat resistant.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 3.80 kg,
Temperature 230 °C
10 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 80 %
80 %
ASTM D638
Flexural Yield Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 5.34 J/cm

@Thickness 6.35 mm
10.0 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
0.25 inch; ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in