Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 70.0 - 245 MPa @Temperature -40.0 - 90.0 °C |
10200 - 35500 psi @Temperature -40.0 - 194 °F |
Average value: 137 MPa Grade Count:2 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Yield Strength | 82.7 - 245 MPa | 12000 - 35500 psi | Average value: 126 MPa Grade Count:14 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Yield Strength | 78.0 - 245 MPa | 11300 - 35500 psi | Average value: 124 MPa Grade Count:18 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |