Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 85.0 - 276 MPa | 12300 - 40000 psi | Average value: 153 MPa Grade Count:12 |
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and .. |
|||
Flexural Yield Strength | 39.0 - 276 MPa | 5660 - 40000 psi | Average value: 101 MPa Grade Count:94 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Flexural Yield Strength | 186 - 276 MPa | 27000 - 40000 psi | Average value: 225 MPa Grade Count:7 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Flexural Yield Strength | 28.0 - 276 MPa | 4060 - 40000 psi | Average value: 92.9 MPa Grade Count:32 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Flexural Yield Strength | 82.7 - 276 MPa | 12000 - 40000 psi | Average value: 184 MPa Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Flexural Yield Strength | 60.0 - 276 MPa @Temperature -40.0 - 150 °C |
8700 - 40000 psi @Temperature -40.0 - 302 °F |
Average value: 150 MPa Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |