Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 110 - 193 MPa | 16000 - 28000 psi | Average value: 142 MPa Grade Count:27 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Flexural Yield Strength | 97.9 - 193 MPa | 14200 - 28000 psi | Average value: 139 MPa Grade Count:24 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Flexural Yield Strength | 82.7 - 193 MPa | 12000 - 28000 psi | Average value: 151 MPa Grade Count:6 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Yield Strength | 13.8 - 193 MPa | 2000 - 28000 psi | Average value: 130 MPa Grade Count:68 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Flexural Yield Strength | 138 - 193 MPa | 20000 - 28000 psi | Average value: 175 MPa Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Flexural Yield Strength | 39.3 - 193 MPa | 5700 - 28000 psi | Average value: 132 MPa Grade Count:100 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Flexural Yield Strength | 138 - 193 MPa | 20000 - 28000 psi | Average value: 175 MPa Grade Count:22 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Flexural Yield Strength | 55.2 - 193 MPa | 8000 - 28000 psi | Average value: 110 MPa Grade Count:28 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |