Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Verton PV007SV_WH8D537 PA 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Verton PV007SV_WH8D537 PA 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Preliminary data for 35% long fiber single pellet color filled PA6This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 175 MPa
25400 psi
Type I, 5 mm/min; ASTM D 638
178 MPa
25800 psi
5 mm/min; ISO 527
Elongation at Break 2.6 %
2.6 %
Type I, 5 mm/min; ASTM D 638
2.8 %
2.8 %
5 mm/min; ISO 527
Tensile Modulus 8.16 GPa
1180 ksi
1 mm/min; ISO 527
9.16 GPa
1330 ksi
5 mm/min; ASTM D 638
Flexural Yield Strength 222 MPa
32200 psi
1.3 mm/min, 50 mm span; ASTM D 790
261 MPa
37900 psi
2 mm/min; ISO 178
Flexural Modulus 6.52 GPa
946 ksi
1.3 mm/min, 50 mm span; ASTM D 790
7.99 GPa
1160 ksi
2 mm/min; ISO 178
Izod Impact, Notched 1.88 J/cm

@Temperature 23.0 °C
3.52 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
2.33 J/cm

@Temperature -40.0 °C
4.37 ft-lb/in

@Temperature -40.0 °F
ASTM D 256
Izod Impact, Unnotched 12.7 J/cm

@Temperature 23.0 °C
23.8 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 19.0 kJ/m²

@Temperature 23.0 °C
9.04 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
27.0 kJ/m²

@Temperature -40.0 °C
12.8 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 82.0 kJ/m²

@Temperature 23.0 °C
39.0 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Users viewing this material also viewed the following: