Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.50 - 14.0 kJ/m² | 4.04 - 6.66 ft-lb/in² | Average value: 11.9 kJ/m² Grade Count:4 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | |
Total Lacqrene® 3351(EU) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180/1A |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | Type 1, Notch A; ISO 180 |
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Polyram PlusTek PA303G4 Nylon 66 for Injection Molding, 20% Glass Fiber Reinforced, Heat Stabilized, Hydrolysis Resistant 20% Glass fiber reinforced, heat stabilized and hydrolysis resistant Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Tisan TISESTER® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Tisan TISESTER® 30% Glass Fiber Reinforced, Flame Retardant (V0). Heat Stabilized. Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF10-66/6-LI6-NBK4 10% Glass Reinforced, Toughened Nylon 66/6 Description: Glass Reinforced, Toughened Nylon 66/6Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF1662-GY1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Polyram RamSter PE321G6 PET, 30% Glass Fiber, Flame Retardant 30% Glass fiber reinforced, flame retardant V-0 PET for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180/1A |
Cathay PA56 Renewable Engineering Polyamide, DAM Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature -40.0 °C |
4.04 ft-lb/in² @Temperature -40.0 °F |
ISO Test |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature -40.0 °C |
4.04 ft-lb/in² @Temperature -40.0 °F |
ISO Test |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl B2I V25 Flame Retardant Nylon 6, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, halogen freeInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180/1A |
Total Lacqrene® 6630 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Izod Impact, Notched (ISO) | 8.50 - 12.0 kJ/m² | 4.04 - 5.71 ft-lb/in² | Average value: 10.2 kJ/m² Grade Count:8 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |