Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 8.50 - 14.0 kJ/m²
4.04 - 6.66 ft-lb/in²
Average value: 11.9 kJ/m² Grade Count:4
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Izod Impact, Notched (ISO) 2.00 - 14.0 kJ/m²

@Temperature -40.0 - -30.0 °C
0.952 - 6.66 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 5.75 kJ/m² Grade Count:5
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched (ISO) 2.00 - 14.0 kJ/m²

@Temperature -40.0 - -30.0 °C
0.952 - 6.66 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 6.80 kJ/m² Grade Count:4
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Izod Impact, Notched (ISO) 3.00 - 14.0 kJ/m²
1.43 - 6.66 ft-lb/in²
Average value: 7.41 kJ/m² Grade Count:39
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Izod Impact, Notched (ISO) 3.00 - 14.0 kJ/m²

@Temperature -30.0 - -30.0 °C
1.43 - 6.66 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.45 kJ/m² Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Izod Impact, Notched (ISO) 12.0 - 14.0 kJ/m²

@Temperature -30.0 - -30.0 °C
5.71 - 6.66 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 13.0 kJ/m² Grade Count:4
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Izod Impact, Notched (ISO) 12.0 - 14.0 kJ/m²

@Thickness 3.20 - 3.20 mm
5.71 - 6.66 ft-lb/in²

@Thickness 0.126 - 0.126 in
Average value: 13.0 kJ/m² Grade Count:4
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Izod Impact, Notched (ISO) 12.0 - 14.0 kJ/m²

@Temperature -30.0 - -30.0 °C
5.71 - 6.66 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 12.6 kJ/m² Grade Count:6
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Izod Impact, Notched (ISO) 12.0 - 14.0 kJ/m²

@Thickness 3.20 - 3.20 mm
5.71 - 6.66 ft-lb/in²

@Thickness 0.126 - 0.126 in
Average value: 12.6 kJ/m² Grade Count:6
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Izod Impact, Notched (ISO) 1.90 - 14.0 kJ/m²

@Temperature -40.0 - -30.0 °C
0.904 - 6.66 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 5.84 kJ/m² Grade Count:3
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Izod Impact, Notched (ISO) 14.0 - 14.0 kJ/m²

@Temperature -30.0 - -30.0 °C
6.66 - 6.66 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 14.0 kJ/m² Grade Count:1
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched (ISO) 3.40 - 14.0 kJ/m²
1.62 - 6.66 ft-lb/in²
Average value: 6.40 kJ/m² Grade Count:4
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..