Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.50 - 9.00 kJ/m² | 4.04 - 4.28 ft-lb/in² | ASTM D256 |
Polikim EFALON® K-25 PTFE, 25% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | |
Total Lacqrene® 3351(EU) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Izod Impact, Notched (ISO) | 8.50 - 57.0 kJ/m² | 4.04 - 27.1 ft-lb/in² | Average value: 18.0 kJ/m² Grade Count:10 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
MBA Polymers PS 3122 Post-consumer recycled impact modified polystyrene Available in standard black.Information provided by MBA Polymers. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | Type 1, Notch A; ISO 180 |
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | Notch A; ISO 180 |
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low .. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Polyram PlusTek PA303G4 Nylon 66 for Injection Molding, 20% Glass Fiber Reinforced, Heat Stabilized, Hydrolysis Resistant 20% Glass fiber reinforced, heat stabilized and hydrolysis resistant Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Tisan TISESTER® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Tisan TISESTER® 30% Glass Fiber Reinforced, Flame Retardant (V0). Heat Stabilized. Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF10-66/6-LI6-NBK4 10% Glass Reinforced, Toughened Nylon 66/6 Description: Glass Reinforced, Toughened Nylon 66/6Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF1662-GY1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GFX1624-BK(PTFE) 30% Glass Fiber Reinforced, Lubricated Nylon 66 Description: Glass Fiber Reinforced, Lubricated Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Polyram RamSter PE321G6 PET, 30% Glass Fiber, Flame Retardant 30% Glass fiber reinforced, flame retardant V-0 PET for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180 |
Total PPC 12712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature -40.0 °C |
4.04 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength stiffness and toughness excellent .. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl A2I V25 Flame Retardant Nylon 66, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, halogen freeInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO Test |
BASF Ultradur B 4300 G3 15% Glass Filled PBT Ultradur B 4300 G3 is an easy flowing injection molding PBT with 15% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO Test |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl B2I V25 Flame Retardant Nylon 6, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, halogen freeInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180/1A |
Total Lacqrene® 6630 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Izod Impact, Notched (ISO) | 8.50 kJ/m² | 4.04 ft-lb/in² | ISO 180/1A |
Total Lacqrene® 6631 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |