Asahi Kasei Thermofil P6-30MI-0533 30% Mica Reinforced, Flame Retardant, Heat Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Mica Filler
Manufacturer Asahi Kasei
Trade Name Thermofil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermofil P6-30MI-0533 30% Mica Reinforced, Flame Retardant, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength, Yield 32.4 MPa
4700 psi
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Strength 48.3 MPa
7000 psi
ASTM D790
Flexural Modulus 5.52 GPa
800 ksi
ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.07 J/cm
2.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
255 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648
Flammability, UL94 V-0
V-0
0.0279 in thickness