Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.00 - 1.51 g/cc
0.0361 - 0.0546 lb/in³
Average value: 1.22 g/cc Grade Count:44
Filler Content 5.00 - 20.0 %
5.00 - 20.0 %
Average value: 10.1 % Grade Count:10
Water Absorption 0.0100 - 0.500 %
0.0100 - 0.500 %
Average value: 0.292 % Grade Count:21
Additive Loading 10.0 - 20.0 %
10.0 - 20.0 %
Average value: 13.8 % Grade Count:4
Linear Mold Shrinkage 0.00300 - 0.0170 cm/cm
0.00300 - 0.0170 in/in
Average value: 0.00566 cm/cm Grade Count:40
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80.0 - 112
80.0 - 112
Average value: 100 Grade Count:3
Tensile Strength, Ultimate 27.6 - 45.0 MPa
4000 - 6530 psi
Average value: 36.4 MPa Grade Count:28
Tensile Strength, Yield 32.4 - 50.3 MPa
4700 - 7300 psi
Average value: 45.9 MPa Grade Count:18
Elongation at Break 1.00 - 10.0 %
1.00 - 10.0 %
Average value: 4.01 % Grade Count:39
Elongation at Yield 1.80 - 4.00 %
1.80 - 4.00 %
Average value: 2.58 % Grade Count:7
Modulus of Elasticity 2.21 - 3.10 GPa
320 - 450 ksi
Average value: 2.66 GPa Grade Count:24
Flexural Yield Strength 8.96 - 89.6 MPa
1300 - 13000 psi
Average value: 68.6 MPa Grade Count:41
Flexural Modulus 1.14 - 6.21 GPa
165 - 900 ksi
Average value: 3.16 GPa Grade Count:42
Izod Impact, Notched 0.267 - 1.60 J/cm
0.500 - 3.00 ft-lb/in
Average value: 0.534 J/cm Grade Count:35
Izod Impact, Unnotched 1.07 - 4.30 J/cm
2.00 - 8.06 ft-lb/in
Average value: 2.12 J/cm Grade Count:30
Izod Impact, Notched (ISO) 4.00 - 7.50 kJ/m²
1.90 - 3.57 ft-lb/in²
Average value: 6.13 kJ/m² Grade Count:4
Izod Impact, Unnotched (ISO) 10.0 - 20.0 kJ/m²
4.76 - 9.52 ft-lb/in²
Average value: 16.0 kJ/m² Grade Count:3
Charpy Impact Unnotched 1.00 - 2.50 J/cm²
4.76 - 11.9 ft-lb/in²
Average value: 1.70 J/cm² Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 66.0 - 84.6 µm/m-°C
36.7 - 47.0 µin/in-°F
Average value: 81.3 µm/m-°C Grade Count:13
CTE, linear, Transverse to Flow 83.0 - 96.0 µm/m-°C
46.1 - 53.3 µin/in-°F
Average value: 90.7 µm/m-°C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 85.0 - 107 °C
185 - 225 °F
Average value: 97.1 °C Grade Count:14
Deflection Temperature at 1.8 MPa (264 psi) 54.4 - 141 °C
130 - 285 °F
Average value: 97.3 °C Grade Count:29
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:26
Electrical Properties Metric English Comments
Electrical Resistivity 0.100 - 1.00e+10 ohm-cm
0.100 - 1.00e+10 ohm-cm
Average value: 2.94e+8 ohm-cm Grade Count:35
Surface Resistance 1.00 - 1.00e+7 ohm
1.00 - 1.00e+7 ohm
Average value: 363000 ohm Grade Count:43
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.38 sec Grade Count:20
Shielding Effectiveness 20.0 - 55.0 dB
20.0 - 55.0 dB
Average value: 42.1 dB Grade Count:14
Processing Properties Metric English Comments
Processing Temperature 210 - 260 °C
410 - 500 °F
Average value: 232 °C Grade Count:5
Melt Temperature 180 - 260 °C
356 - 500 °F
Average value: 229 °C Grade Count:19
Mold Temperature 38.0 - 93.3 °C
100 - 200 °F
Average value: 69.8 °C Grade Count:22
Drying Temperature 70.0 - 95.0 °C
158 - 203 °F
Average value: 81.2 °C Grade Count:20
Moisture Content 0.0200 - 0.100 %
0.0200 - 0.100 %
Average value: 0.0893 % Grade Count:15
Dew Point -17.8 °C
0.000 °F
Average value: -17.8 °C Grade Count:13
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:16