Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.60 - 6.94 J/cm | 3.00 - 13.0 ft-lb/in | Average value: 3.72 J/cm Grade Count:36 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Unnotched | 3.74 - 6.94 J/cm | 7.00 - 13.0 ft-lb/in | Average value: 5.31 J/cm Grade Count:19 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Unnotched | 4.27 - 6.94 J/cm | 8.00 - 13.0 ft-lb/in | Average value: 6.10 J/cm Grade Count:5 |
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Izod Impact, Unnotched | 4.81 - 6.94 J/cm | 9.00 - 13.0 ft-lb/in | Average value: 5.61 J/cm Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Izod Impact, Unnotched | 1.07 - 6.94 J/cm | 2.00 - 13.0 ft-lb/in | Average value: 3.89 J/cm Grade Count:35 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Izod Impact, Unnotched | 3.74 - 6.94 J/cm | 7.00 - 13.0 ft-lb/in | Average value: 5.15 J/cm Grade Count:24 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Izod Impact, Unnotched | 3.35 - 6.94 J/cm | 6.28 - 13.0 ft-lb/in | Average value: 5.18 J/cm Grade Count:9 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Izod Impact, Unnotched | 3.74 - 6.94 J/cm | 7.00 - 13.0 ft-lb/in | Average value: 4.68 J/cm Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |