Material Notes:
Information provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Tensile Modulus 2.00 GPa
290 ksi
ASTM D638
Flexural Yield Strength 85.15 MPa
12350 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Unnotched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Falling Dart Impact 36.6 J
27.0 ft-lb
73°F; ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 74.9 µm/m-°C

@Temperature 20.0 °C
41.6 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Gloss 85 %
85 %
Gardner; ASTM D2523