Polymer Property : Izod Impact, Notched = 3.50 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.17 - 1.87 J/cm
2.20 - 3.50 ft-lb/in
Average value: 1.49 J/cm Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
Izod Impact, Notched 1.66 - 1.87 J/cm
3.10 - 3.50 ft-lb/in
Average value: 1.77 J/cm Grade Count:3
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Izod Impact, Notched 0.370 - 1.87 J/cm
0.693 - 3.50 ft-lb/in
Average value: 0.799 J/cm Grade Count:19
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Izod Impact, Notched 0.534 - 1.87 J/cm
1.00 - 3.50 ft-lb/in
Average value: 1.25 J/cm Grade Count:44
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Notched 0.214 - 1.87 J/cm
0.401 - 3.50 ft-lb/in
Average value: 0.968 J/cm Grade Count:124
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Notched 1.33 - 1.87 J/cm
2.50 - 3.50 ft-lb/in
ASTM D256
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Izod Impact, Notched 0.883 - 1.87 J/cm
1.65 - 3.50 ft-lb/in
Average value: 1.38 J/cm Grade Count:14
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
Izod Impact, Notched 0.534 - 1.87 J/cm
1.00 - 3.50 ft-lb/in
Average value: 1.27 J/cm Grade Count:38
Overview of materials for Polycarbonate, 40% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E..
Izod Impact, Notched 0.480 - 1.87 J/cm

@Temperature -40.0 - 0.000 °C
0.899 - 3.50 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 0.922 J/cm Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Izod Impact, Notched 0.480 - 1.87 J/cm

@Thickness 3.17 - 3.20 mm
0.899 - 3.50 ft-lb/in

@Thickness 0.125 - 0.126 in
Average value: 0.922 J/cm Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Izod Impact, Notched 0.267 - 1.87 J/cm
0.500 - 3.50 ft-lb/in
Average value: 0.622 J/cm Grade Count:42
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..