Polymer Property : Izod Impact, Notched = 1.33 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.33 J/cm

@Temperature 23.0 °C
2.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products RCC233-01 33% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: Fender linersSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
73°F; ASTM D256
Ravago Manufacturing Americas Hylon® N1043L Nylon 6/6 (DAM)
Information provided by Ravago.
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS (Europe-Africa-Middle East)
LNP* Lubricomp* Cycoloy_C2801 compound is a 5% PTFE reinforced PC+ABS wear resistant flame retardant resin for moving components in business equipment. Medium heat performance
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin  (discontinued **)
Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i..
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 205D TFE 15  Nylon 6/12 (PA 6/12) Glass Fiber 30% - PTFE 15%  (discontinued
Glass Fiber 30% - PTFE 15%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provide..
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Asia Pacific)
LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.
Izod Impact, Notched 1.33 J/cm

@Temperature -30.0 °C
2.49 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA
Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance.
Izod Impact, Notched 1.33 J/cm

@Temperature -40.0 °C
2.49 ft-lb/in

@Temperature -40.0 °F
ASTM D256
SABIC Innovative Plastics NORYL PX1391 PPE+PS (Asia Pacific)
Automotive applications, primarily. Excellent electrical properties. high heat. 305F (152C) DTUL.
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC
LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing 20% Glass Fiber.
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM Data
Styron Magnumâ„¢ 347EZ ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Izod Impact, Notched 1.33 J/cm

@Temperature 22.8 °C
2.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Teknor Apex Chemlon® 143 G Nylon 66, 43% Short Glass Fiber Reinforced
Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Chase Plastics CP Pryme® PC110GR Polycarbonate, 10% Glass Fiber Reinforced, Mold Release
Information provided by Chase Plastics.
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Izod Impact, Notched 1.33 J/cm

@Thickness 3.20 mm
2.50 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company ESD 3284 Ethylene Tetrafluoroethylene (ETFE) Carbon Fiber - Electrically Conductive
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 2385 A HEC UV Rigid Thermoplastic Polyurethane (RTPU), Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection - UV Stabilized
Izod Impact, Notched 1.33 J/cm

@Thickness 3.20 mm
2.50 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company RTP 199 X 135006 A Polypropylene (PP) Glass Fiber - Flame Retardant - Non-PBB/PBDE
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ PP 1579 Impact Grade Polypropylene
DescriptionPolyfort® PP 1579H is an impact grade of polypropylene for use in parts which require good impact and good appearance in light-weight injection molded parts. Information provided by A. ..
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 2205 LF TFE 15 Z Polyetheretherketone (PEEK), Glass Fiber - PTFE Lubricated - FDA Compliant Ingredients
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
2.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Diamond Polymers ABS 1501E
Description: Extrusion GradeInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 1.33 J/cm

@Temperature 22.8 °C
2.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant Renol PA2SP0017 Nylon 6, Impact Modified
Data provided by Clariant Masterbatches
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Copolymer CP0437G5M25CL Glass/Mineral Reinforced Coupled
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Bapolene® PP5062 Polypropylene, Injection Grade
Polypropylene injection impact copolymer with excellent color and processability. This resin offers a superior balance of stiffness and impact strength. This product meets the FDA requirements of ..
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
A. Schulman ComAlloy Comtuf® 630 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int..
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
Wet; ASTM D256
Asahi Kasei Leona® 90G50 50% Glass Filled Nylon 66
Enhanced strength and stiffness; with 50% GF. Excellent appearance.Applications:Office furnitureInformation provided by Asahi Kasei
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Omni Plastics OmniTuff™ CPP GRC20 Copolymer Polypropylene Glass Reinforced
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
2.49 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Ravago Manufacturing Americas Hylex® P1310G40 HB Polycarbonate, 40% Fiberglass Reinforced, UV Stabilized
Information provided by Ravago.
Izod Impact, Notched 1.33 J/cm

@Thickness 3.20 mm
2.50 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company RTP 299 M X 122533 Nylon 1010; Carbon Fiber Reinforced - PTFE Lubricated - Wear Resistant
Izod Impact, Notched 1.33 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Edgetek® AM 33 GF/000 L HS Black Polyphthalamide (PPA), Glass Filled  (discontinued **)
Description/Features:Heat StabilizedBlackEnhanced LubricationGlass Fiber ReinforcedInformation provided by PolyOne Corporation.
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
ASTM D 256
RTP Company RTP 206 B Nylon 6/10 (PA), Glass Fiber
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 303 FR UV Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E - UV Stabilized
The RTP series of flame retardant, glass fiber reinforced polycarbonate materials offer dimensional stability with improved heat distortion and ignition resistance performance over the base resin. ..