Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Amco Amalloy® B1025 Polymer Alloy

Category Polymer , Thermoplastic
Manufacturer Amco Plastic Materials
Trade Name Amalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amco Amalloy® B1025 Polymer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amco Amalloy B1025 is a clear performance copolymer with exceptional clarity and toughness.Clear, medium melt-flow.Information provided by Amco Plastic Materials.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D1505
Melt Flow 5.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D638
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 103 °C
217 °F
ASTM D648
Optical Properties Metric English Comments
Haze 1.7 %

@Thickness 2.54 mm
1.7 %

@Thickness 0.100 in
ASTM D1003
Transmission, Visible 90.2 %

@Thickness 2.54 mm
90.2 %

@Thickness 0.100 in
ASTM D1003
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved