Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.187 - 0.694 J/cm | 0.350 - 1.30 ft-lb/in | Average value: 0.388 J/cm Grade Count:4 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 0.214 - 0.694 J/cm | 0.400 - 1.30 ft-lb/in | Average value: 0.409 J/cm Grade Count:59 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.374 - 0.694 J/cm | 0.700 - 1.30 ft-lb/in | Average value: 0.502 J/cm Grade Count:10 |
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Izod Impact, Notched | 0.320 - 0.694 J/cm | 0.600 - 1.30 ft-lb/in | Average value: 0.495 J/cm Grade Count:18 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched | 0.694 - 0.694 J/cm @Temperature -40.0 - -40.0 °C |
1.30 - 1.30 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.694 J/cm Grade Count:1 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |