Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.21 - 2.17 g/cc
0.0437 - 0.0784 lb/in³
Average value: 1.50 g/cc Grade Count:256
Filler Content 5.00 - 40.0 %
5.00 - 40.0 %
Average value: 20.6 % Grade Count:62
Water Absorption 0.100 - 2.20 %
0.100 - 2.20 %
Average value: 0.539 % Grade Count:141
Moisture Absorption at Equilibrium 0.0200 - 1.00 %
0.0200 - 1.00 %
Average value: 0.529 % Grade Count:48
Additive Loading 10.0 - 40.0 %
10.0 - 40.0 %
Average value: 27.8 % Grade Count:9
Viscosity 80.0 - 1450 cP
80.0 - 1450 cP
Average value: 632 cP Grade Count:10
Viscosity Test 48.0 - 82.0 cm³/g
48.0 - 82.0 cm³/g
Average value: 60.0 cm³/g Grade Count:7
Linear Mold Shrinkage 0.000100 - 0.0100 cm/cm
0.000100 - 0.0100 in/in
Average value: 0.00414 cm/cm Grade Count:227
Linear Mold Shrinkage, Transverse 0.00250 - 0.0300 cm/cm
0.00250 - 0.0300 in/in
Average value: 0.00686 cm/cm Grade Count:60
Melt Flow 4.50 - 150 g/10 min
4.50 - 150 g/10 min
Average value: 39.0 g/10 min Grade Count:40
Mechanical Properties Metric English Comments
Hardness, Rockwell M 98.0
98.0
Average value: 98.0 Grade Count:3
Hardness, Rockwell R 98.0 - 127
98.0 - 127
Average value: 121 Grade Count:40
Ball Indentation Hardness 154 - 224 MPa
22300 - 32500 psi
Average value: 174 MPa Grade Count:12
Tensile Strength, Ultimate 25.0 - 325 MPa
3630 - 47100 psi
Average value: 114 MPa Grade Count:222
10.0 - 135 MPa

@Temperature 60.0 - 150 °C
1450 - 19600 psi

@Temperature 140 - 302 °F
Average value: 68.8 MPa Grade Count:4
31.0 - 43.0 MPa

@Temperature 180 - 180 °C
4500 - 6240 psi

@Temperature 356 - 356 °F
Average value: 68.8 MPa Grade Count:1
31.0 - 43.0 MPa

@# of Cycles 100000 - 1.00e+7
4500 - 6240 psi

@# of Cycles 100000 - 1.00e+7
Average value: 68.8 MPa Grade Count:1
23.0 - 80.0 MPa

@Temperature 160 - 160 °C
3340 - 11600 psi

@Temperature 320 - 320 °F
Average value: 68.8 MPa Grade Count:2
23.0 - 80.0 MPa

@Strain 0.600 - 3.00 %
3340 - 11600 psi

@Strain 0.600 - 3.00 %
Average value: 68.8 MPa Grade Count:2
Tensile Strength, Yield 60.0 - 221 MPa
8700 - 32000 psi
Average value: 107 MPa Grade Count:55
50.0 - 75.0 MPa

@Temperature 60.0 - 140 °C
7250 - 10900 psi

@Temperature 140 - 284 °F
Average value: 63.3 MPa Grade Count:1
Elongation at Break 0.450 - 100 %
0.450 - 100 %
Average value: 5.75 % Grade Count:203
2.10 - 20.0 %

@Temperature 60.0 - 150 °C
2.10 - 20.0 %

@Temperature 140 - 302 °F
Average value: 28.3 % Grade Count:4
Elongation at Yield 0.189 - 8.00 %
0.189 - 8.00 %
Average value: 3.03 % Grade Count:67
2.50 - 5.50 %

@Temperature 60.0 - 150 °C
2.50 - 5.50 %

@Temperature 140 - 302 °F
Average value: 3.85 % Grade Count:3
Modulus of Elasticity 2.00 - 36.6 GPa
290 - 5300 ksi
Average value: 7.77 GPa Grade Count:226
2.25 - 10.0 GPa

@Temperature 60.0 - 160 °C
326 - 1450 ksi

@Temperature 140 - 320 °F
Average value: 5.59 GPa Grade Count:7
Flexural Yield Strength 2.60 - 310 MPa
377 - 45000 psi
Average value: 170 MPa Grade Count:226
Flexural Modulus 2.00 - 24.1 GPa
290 - 3500 ksi
Average value: 7.17 GPa Grade Count:230
Compressive Yield Strength 100 - 241 MPa
14500 - 35000 psi
Average value: 133 MPa Grade Count:25
Fatigue Strength 5.00 - 12.0 MPa

@# of Cycles 10000 - 1.00e+7
725 - 1740 psi

@# of Cycles 10000 - 1.00e+7
Average value: 8.25 MPa Grade Count:1
5.00 - 12.0 MPa

@Temperature 180 - 180 °C
725 - 1740 psi

@Temperature 356 - 356 °F
Average value: 8.25 MPa Grade Count:1
Shear Modulus 0.200 - 1.00 GPa

@Temperature 50.0 - 225 °C
29.0 - 145 ksi

@Temperature 122 - 437 °F
Average value: 0.762 GPa Grade Count:7
Izod Impact, Notched 0.214 - 2.14 J/cm
0.400 - 4.00 ft-lb/in
Average value: 0.673 J/cm Grade Count:190
Izod Impact, Unnotched 1.87 - 5340 J/cm
3.50 - 10000 ft-lb/in
Average value: 6.03 J/cm Grade Count:136
Izod Impact, Notched (ISO) 4.00 - 15.7 kJ/m²
1.90 - 7.49 ft-lb/in²
Average value: 6.94 kJ/m² Grade Count:67
5.00 - 14.7 kJ/m²

@Temperature -30.0 - 120 °C
2.38 - 6.99 ft-lb/in²

@Temperature -22.0 - 248 °F
Average value: 8.02 kJ/m² Grade Count:8
Izod Impact, Unnotched (ISO) 6.50 kJ/m² - NB
3.09 ft-lb/in² - NB
Average value: 38.8 kJ/m² Grade Count:57
42.0 - 59.0 kJ/m²

@Temperature -25.0 - 120 °C
20.0 - 28.1 ft-lb/in²

@Temperature -13.0 - 248 °F
Average value: 52.7 kJ/m² Grade Count:1
Charpy Impact Unnotched 1.90 J/cm² - NB
9.04 ft-lb/in² - NB
Average value: 4.44 J/cm² Grade Count:32
4.50 J/cm² - NB

@Temperature -30.0 - -20.0 °C
21.4 ft-lb/in² - NB

@Temperature -22.0 - -4.00 °F
Average value: 4.50 J/cm² Grade Count:10
Charpy Impact, Notched 0.350 - 1.00 J/cm²
1.67 - 4.76 ft-lb/in²
Average value: 0.676 J/cm² Grade Count:31
0.250 - 0.800 J/cm²

@Temperature -30.0 - -20.0 °C
1.19 - 3.81 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.636 J/cm² Grade Count:11
Dart Drop, Total Energy 4.00 - 19.0 J
2.95 - 14.0 ft-lb
Average value: 11.8 J Grade Count:26
Falling Dart Impact 4.20 - 12.8 J
3.10 - 9.44 ft-lb
Average value: 9.27 J Grade Count:4
Coefficient of Friction 0.200 - 0.520
0.200 - 0.520
Average value: 0.363 Grade Count:19
Coefficient of Friction, Static 0.120 - 0.630
0.120 - 0.630
Average value: 0.329 Grade Count:19
Tensile Creep Modulus, 1000 hours 2700 - 8300 MPa
392000 - 1.20e+6 psi
Average value: 3760 MPa Grade Count:8
K (wear) Factor 8.06 - 342 x 10-8 mm³/N-M
4.00 - 170 x 10-10 in³-min/ft-lb-hr
Average value: 105 x 10<sup>-8</sup> mm³/N-M Grade Count:13
Electrical Properties Metric English Comments
Electrical Resistivity 6.60 - 1.00e+17 ohm-cm
6.60 - 1.00e+17 ohm-cm
Average value: 9.88e+15 ohm-cm Grade Count:124
Surface Resistance 2.00 - 1.00e+15 ohm
2.00 - 1.00e+15 ohm
Average value: 5.79e+13 ohm Grade Count:39
Insulation Resistance 100000 - 1.00e+12 ohm
100000 - 1.00e+12 ohm
Average value: 6.88e+11 ohm Grade Count:16
Static Decay 1.00 - 2.00 sec
1.00 - 2.00 sec
Average value: 1.80 sec Grade Count:10
Dielectric Constant 3.10 - 4.30
3.10 - 4.30
Average value: 3.76 Grade Count:55