Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem CP360H Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem CP360H Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Narrow MWD, Low Smoke / CondensateApplications: Suggested Uses Include Fine Denier Spunbond Nonwovens, High-Speed Spinning - Continuous Filament YarnThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 34 g/10 min

@Load 2.16 kg,
Temperature 230 °C
34 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ASTM D785
Tensile Strength 32.4 MPa
4700 psi
2 in/min; ASTM D638
Elongation at Yield 11 %
11 %
2 in/min; ASTM D638
Tenacity 0.203 N/tex
2.30 g/denier
3.3 draw ration, 1,250 m/min roll speed; 225°C spin temperature, D1000/68, ASTM D2256
Flexural Modulus 1.17 GPa
170 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256A
Descriptive Properties Value Comments
Elongation of Fibers (3.3 draw ration, 1,250 m/min roll speed) 117%
225°C spin temperature, D1000/68, ASTM D2256
Suggested Takeup Roll Speed 13122 ft/min
Copyright © lookpolymers.com All Rights Reserved