Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.694 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.187 - 0.694 J/cm
0.350 - 1.30 ft-lb/in
Average value: 0.388 J/cm Grade Count:4
Overview of materials for Epoxy Encapsulant, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o..
Izod Impact, Notched 0.214 - 0.694 J/cm
0.400 - 1.30 ft-lb/in
Average value: 0.409 J/cm Grade Count:59
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Notched 0.374 - 0.694 J/cm
0.700 - 1.30 ft-lb/in
Average value: 0.502 J/cm Grade Count:10
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma..
Izod Impact, Notched 0.320 - 0.694 J/cm
0.600 - 1.30 ft-lb/in
Average value: 0.495 J/cm Grade Count:18
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
Izod Impact, Notched 0.694 - 0.694 J/cm

@Temperature -40.0 - -40.0 °C
1.30 - 1.30 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.694 J/cm Grade Count:1
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and ..